Sign Up to like & get
recommendations!
1
Published in 2019 at "Applied Surface Science"
DOI: 10.1016/j.apsusc.2018.08.255
Abstract: Abstract Highly ordered As/Si faceted lateral nanoprisms array with a uniform width of about 10–18 nm are fabricated on Si {1 0 3} miscut surface via thermal deposition of sub-monolayer arsenic followed by a subsequent annealing process. In…
read more here.
Keywords:
lateral nanoprisms;
surface;
arsenic induced;
faceted lateral ... See more keywords