Applying Machine Learning to Nanoindentation Data of (Nano-) Enhanced Composites

Sign Up to like & get
recommendations!
Published in 2019 at "Fibers"

DOI: 10.3390/fib8010003

Abstract: Carbon fiber reinforced polymers (CFRPs) are continuously gaining attention in aerospace and space applications, and especially their multi-scale reinforcement with nanoadditives. Carbon nanotubes (CNTs), graphene, carbon nanofibers (CNFs), and their functionalized forms are often incorporated… read more here.