Published in 2017 at "Corrosion Science"
DOI: 10.1016/j.corsci.2016.11.017
Abstract: Lithium deuteride (LiD) was exposed to air for 600 min to determine the effect of air humidity on its microstructure and phase composition. XRD and XPS results revealed that LiOH and Li2CO3 formed at relative humidity…