Published in 2017 at "Journal of Applied Polymer Science"
DOI: 10.1002/app.44559
Abstract: The mechanical properties of ferromagnetic particle-reinforced silicone–rubber matrix composites are examined with quasi-static and dynamic nanoindentation measurements using Berkovich and flat punch indenters, respectively. Quasi-static nanoindentation is performed to examine primary factors such as the…
read more here.
Keywords:
dynamic nanoindentation;
quasi static;
soft composites;
particle ... See more keywords
Photo by nci from unsplash
Sign Up to like & get
recommendations!
1
Published in 2022 at "Methods in molecular biology"
DOI: 10.1007/978-1-0716-1816-5_6
Abstract: Growth and morphogenesis in plants depend on cell wall mechanics and on turgor pressure. Nanoindentation methods, such as atomic force microscopy (AFM), enable measurements of mechanical properties of a tissue at subcellular resolution, while confocal…
read more here.
Keywords:
cell mechanics;
microscopy;
plugin;
nanoindentation ... See more keywords
Photo from archive.org
Sign Up to like & get
recommendations!
2
Published in 2019 at "Methods in molecular biology"
DOI: 10.1007/978-1-4939-8894-5_14
Abstract: Proteinaceous assemblies are ubiquitous in nature. One important form of these assemblies are protein nanoshells such as viruses; however, a variety of other protein shells exist. To deepen our knowledge on the structure and function…
read more here.
Keywords:
nanoindentation experiments;
protein shells;
shells protocol;
experiments protein ... See more keywords
Photo from wikipedia
Sign Up to like & get
recommendations!
1
Published in 2020 at "European Journal of Wood and Wood Products"
DOI: 10.1007/s00107-020-01520-1
Abstract: The performance of adhesive-hardwood bonds can often be sensitive to humidity and temperature variation. Therefore, it is frequently challenging to achieve standard requirements for structural applications. To gain a better understanding of the wood-adhesive bond,…
read more here.
Keywords:
wood adhesive;
shear strength;
wet conditions;
nanoindentation ... See more keywords
Photo from wikipedia
Sign Up to like & get
recommendations!
1
Published in 2017 at "Acta Mechanica"
DOI: 10.1007/s00707-017-1901-9
Abstract: In the present paper, the nanoindentation of an elastic half-space by a conical indenter is investigated with the influence of surface tension. Based on the solution of a point force acting on an elastic half-space…
read more here.
Keywords:
tension;
nanoindentation;
surface tension;
conical indenter ... See more keywords
Sign Up to like & get
recommendations!
0
Published in 2017 at "Tribology Letters"
DOI: 10.1007/s11249-017-0950-5
Abstract: Abstract304 Stainless steel (SS)-reinforced A356 aluminium matrix composites were manufactured by melt infiltration casting. Recycled SS shavings were pressed to obtain porous monoblock preform, and molten Al alloy was infiltrated into vacancies of the preform…
read more here.
Keywords:
aluminium matrix;
wear;
steel reinforced;
stainless steel ... See more keywords
Sign Up to like & get
recommendations!
0
Published in 2017 at "JOM"
DOI: 10.1007/s11837-017-2541-1
Abstract: Nanoindentation is a hardness test method applied to small volumes of material which can provide some unique effects and spark many related research activities. To fully understand the phenomena observed during nanoindentation tests, modeling and…
read more here.
Keywords:
simulation nanoindentation;
modeling simulation;
nanoindentation;
Photo from wikipedia
Sign Up to like & get
recommendations!
1
Published in 2018 at "JOM"
DOI: 10.1007/s11837-018-2850-z
Abstract: Hydrogen effects on small-volume plasticity and elastic stiffness constants are investigated with nanoindentation of Ni-201 and sonic velocity measurements of bulk Ni single crystals. Elastic modulus of Ni-201, calculated from indentation data, decreases ~ 22% after…
read more here.
Keywords:
hydrogen;
deformation;
nanoindentation;
plastic deformation ... See more keywords
Photo from wikipedia
Sign Up to like & get
recommendations!
0
Published in 2017 at "Metals and Materials International"
DOI: 10.1007/s12540-017-6461-y
Abstract: Nanoindentation has been widely used to measure mechanical properties for instance elastic modulus and hardness due to relatively simple sample preparation and experimental procedure. Primary limitation of nanoindentation is that it does not measure quantitative…
read more here.
Keywords:
strain;
stress strain;
electroplated copper;
nanoindentation ... See more keywords
Photo from wikipedia
Sign Up to like & get
recommendations!
0
Published in 2017 at "Electronic Materials Letters"
DOI: 10.1007/s13391-017-6348-6
Abstract: AbstractIn this paper the effect of hydrogen implantation in silicon on nanoindentation-induced phase transformation is investigated. Hydrogen ions were implanted in silicon through 300 nm thick oxide with double energy implantation (75 and 40 keV).…
read more here.
Keywords:
hydrogen;
nanoindentation;
induced phase;
spectroscopy ... See more keywords
Photo from wikipedia
Sign Up to like & get
recommendations!
0
Published in 2018 at "Applied Surface Science"
DOI: 10.1016/j.apsusc.2017.10.106
Abstract: Abstract This paper proposes a correction method to accurately evaluate the nanoindentation load-depth ( P-h ) curve of MEMS double clamped micro bridge structures. Critical elastic and plastic deflections of the bent bridge are extracted…
read more here.
Keywords:
micro bridge;
depth;
bridge;
nanoindentation ... See more keywords