Published in 2018 at "Micromachines"
DOI: 10.3390/mi9100518
Abstract: The nanomechanical properties and nanoindentation responses of bismuth selenide (Bi2Se3) thin films are investigated in this study. The Bi2Se3 thin films are deposited on c-plane sapphire substrates using pulsed laser deposition. The microstructural properties of…
read more here.
Keywords:
nanoindentation bi2se3;
bi2se3 thin;
thin films;