A study of the nanoindentation creep behavior of (La0.5Ce0.5)65Al10Co25 metallic glass based on fractional differential rheological model

Sign Up to like & get
recommendations!
Published in 2018 at "Journal of Non-crystalline Solids"

DOI: 10.1016/j.jnoncrysol.2018.03.045

Abstract: Abstract A fractional differential rheological model was proposed to describe the nanoindentation creep behavior of metallic glasses (MGs) at room temperature. The model had been proved to not only include the conventional rheological model, but… read more here.