Nanoindentation investigation on creep behavior of amorphous CuZrAl/nanocrystalline Cu nanolaminates

Sign Up to like & get
recommendations!
Published in 2017 at "Journal of Non-crystalline Solids"

DOI: 10.1016/j.jnoncrysol.2017.03.037

Abstract: Abstract Berkovich nanoindentation experiments have been performed on amorphous /nanocrystalline nanolaminates with individual Cu Zr Al layers (45 nm, 90 nm, 225 nm) and Cu layers (7.5 nm & 15 nm). Elastic modulus, hardness and indentation morphology were detected and… read more here.

Keywords: investigation creep; nanocrystalline nanolaminates; nanocrystalline; creep deformation ... See more keywords