Sign Up to like & get
recommendations!
1
Published in 2017 at "Ferroelectrics"
DOI: 10.1080/00150193.2017.1367226
Abstract: ABSTRACT In this work, the poled PVDF with metal coating was prepared. The microscopy characterization and crystalline phase were studied. The piezoresponse force microscope (PFM) test, nanoindentation and nanoscratch tests were carried out. The focus…
read more here.
Keywords:
nanoindentation nanoscratch;
pvdf sheet;
sheet;
poled pvdf ... See more keywords
Sign Up to like & get
recommendations!
0
Published in 2019 at "Advances in Materials and Processing Technologies"
DOI: 10.1080/2374068x.2019.1578554
Abstract: ABSTRACT Aluminium matrix nanocomposites reinforced with 0.5 and 1wt% functionalized graphene nanoplatelets were fabricated via spark plasma sintering (SPS). Nanoindentation and nanoscratch tests were performed on the nanocomposites to evaluate the mechanical and tribological properties…
read more here.
Keywords:
spark plasma;
graphene nanoplatelets;
aluminium;