Published in 2019 at "JOM"
DOI: 10.1007/s11837-019-03860-7
Abstract: The results of high-temperature nanoindentation testing on both a control and a neutron-irradiated silicon carbide matrix silicon carbide fiber composite sample are presented. The mechanical properties of the chemical vapor-infiltrated matrix were observed to have…