AFM Nanoindentation of Stiff Inhomogeneous Layer on Polymeric Substrate

Sign Up to like & get
recommendations!
Published in 2024 at "Microscopy Research and Technique"

DOI: 10.1002/jemt.24734

Abstract: Analysis of indentation data of heterogeneous material, in particular, layer on an elastic substrate requires information about the contact area that is essential for calculating mechanical properties. The actual shape of the AFM‐tip is not… read more here.

Keywords: layer; indentation; afm nanoindentation; nanoindentation stiff ... See more keywords