Published in 2020 at "International Journal of Refractory Metals and Hard Materials"
DOI: 10.1016/j.ijrmhm.2020.105222
Abstract: Abstract Knowledge of mechanical properties of the tungsten surface region is extremely important for its application as first wall materials in plasma-facing components for nuclear fusion devices (e.g. ITER). Since tungsten is intrinsically brittle at…
read more here.