Nanoindentation of ZrH2 by molecular dynamics simulation

Sign Up to like & get
recommendations!
Published in 2020 at "Journal of Nuclear Materials"

DOI: 10.1016/j.jnucmat.2020.152391

Abstract: Abstract Classical molecular dynamics simulations of nanoindentation on the (100) and (110) planes using a spherical indenter are performed to investigate the deformation behavior of δ -ZrH2. The Charged Optimized Many Body (COMB) potential is… read more here.