A Study on Microstructural Evolution in Cold Rotary Forged Nickel-Superalloys: C263 and Inconel 718

Sign Up to like & get
recommendations!
Published in 2020 at "Procedia Manufacturing"

DOI: 10.1016/j.promfg.2020.04.296

Abstract: Abstract C263 and Inconel 718 are precipitation hardenable nickel-superalloys widely used in different sections of a gas turbine engine dependent on their strength and temperature capability. Cold rotary forging is an effective route for manufacturing… read more here.

Keywords: nickel superalloys; forging; cold rotary; c263 inconel ... See more keywords