Articles with "oxide scales" as a keyword



The Effect of Temperature on the Formation of Oxide Scales Regarding Commercial Superheater Steels

Sign Up to like & get
recommendations!
Published in 2017 at "Oxidation of Metals"

DOI: 10.1007/s11085-017-9785-6

Abstract: This study addresses the surface changes of three commercial steels (a low alloy ferritic 10CrMo9-10 steel, a Nb-stabilized austenitic AISI347 steel, and a high alloy austenitic Sanicro 28 steel) by comparing the oxide scale thicknesses,… read more here.

Keywords: oxide scales; temperature; effect temperature; effect ... See more keywords

Enhanced plasticity of the oxide scales by in-situ formed Cr2O3/Cr heterostructures for Cr-based coatings on Zr alloy in 1200 °C steam

Sign Up to like & get
recommendations!
Published in 2021 at "Corrosion Science"

DOI: 10.1016/j.corsci.2021.109361

Abstract: Abstract The mechanical maintenance of oxides scales was studied for the chromium (Cr) coated zirconium (Zr) alloy coupons that proceeded oxidation in the 1200 °C steam. During the oxidation process, Cr/CrAlSiN coatings evolved into a… read more here.

Keywords: 1200 steam; oxide scales; plasticity oxide; scales situ ... See more keywords
Photo from academic.microsoft.com

Room temperature plasticity in thermally grown sub-micron oxide scales revealed by micro-cantilever bending

Sign Up to like & get
recommendations!
Published in 2018 at "Scripta Materialia"

DOI: 10.1016/j.scriptamat.2017.09.036

Abstract: We propose a new geometry for focused ion beam milled micro-cantilevers, which allows production of residual stress-free, isolated thin film specimens from film-substrate systems. This geometry was used to demonstrate the presence of permanent deformation… read more here.

Keywords: temperature plasticity; oxide scales; thermally grown; room temperature ... See more keywords

High-Temperature Corrosion Behavior of Superheater Materials at 600 °C: Insights from Laboratory and Field Exposures

Sign Up to like & get
recommendations!
Published in 2024 at "Energy & Fuels"

DOI: 10.1021/acs.energyfuels.4c04806

Abstract: Combustion of biomass and waste results in release of corrosive species, such as alkali chlorides and water vapor, which accelerate the corrosion of superheaters in the boiler. To improve our understanding of alkali-induced corrosion, long-term… read more here.

Keywords: corrosion behavior; oxides outer; oxide scales; rich oxides ... See more keywords