Published in 2025 at "International Journal of Applied Ceramic Technology"
DOI: 10.1111/ijac.70001
Abstract: Pressureless sintering of Si3N4 doped with 2 mol% Y2O3 and 5 mol% MgO was carried out at temperatures ranging from 1700°C to 1770°C in three kinds of packing powders consisting of Si3N4 and BN coupled with or…
read more here.
Keywords:
packing powder;
thermal conductivity;
powder;
densification ... See more keywords