Published in 2020 at "Metallurgical and Materials Transactions B"
DOI: 10.1007/s11663-020-01893-x
Abstract: The partial roasting of high-arsenic copper concentrates at 973 K/998 K (700 °C/725 °C) under controlled atmosphere can remove > 95 pct of the arsenic contained in the concentrates, leaving a calcine with 52 to 68 wt pct bornite, 10 to 13 wt pct…