Published in 2018 at "Kinetics and Catalysis"
DOI: 10.1134/s0023158418010068
Abstract: It is established that the main regularities of the peroxide delignification of aspen wood in the temperature range of 70–100°С in the presence of dissolved (H2SO4) and solid (TiO2) catalysts are similar. With an increase…
read more here.
Keywords:
cellulose products;
peroxide delignification;
delignification aspen;
aspen wood ... See more keywords