Published in 2020 at "Rare Metals"
DOI: 10.1007/s12598-020-01400-w
Abstract: The Ni–Co–Cr–W–Mo system is critical for the design of nickel-based superalloys. This system stabilizes different topologically close-packed (TCP) phases in many commercially superalloys with high W and Mo contents. Scanning electron microscopy (SEM), transmission electron…