Published in 2023 at "Ferroelectrics"
DOI: 10.1080/00150193.2023.2189826
Abstract: Abstract Pure Li2MnO3 powders were synthesized at 900 °C for 4 h by a solid-state reaction method. Li2MnO3 ceramics were prepared in the temperature range of 1100 °C to 1250 °C. All the samples displayed a single phase structure.…