Sign Up to like & get
recommendations!
1
Published in 2018 at "International Journal of Fatigue"
DOI: 10.1016/j.ijfatigue.2017.09.020
Abstract: Abstract The micro arc oxidation (MAO) coatings of 50 ± 5 µm thickness were deposited on 6061-T6 Al alloy substrates with and without prior shot peening. The peening was carried out using 3-different shot materials namely cast…
read more here.
Keywords:
shot peening;
6061 alloy;
prior shot;
fatigue life ... See more keywords