Abstract: High Fe levels, coarse grains, microstructural inhomogeneities, and coarse dispersoids for recrystallization suppression remain problems for industrial application of Al–Mg–Si (6xxx) alloys. Herein, Al–0.81%Mg–0.81%Si–0.7%Fe alloy billets are fabricated by direct chill (DC) casting at different…