Published in 2020 at "Journal of The European Ceramic Society"
DOI: 10.1016/j.jeurceramsoc.2020.01.048
Abstract: Abstract The brittleness of MoSi2 ceramic and the thermal mismatch between MoSi2 coating and C / C composite lead to brittle cracking of the coating at 900−1200 °C. This problem has been overcome in this studyby…
read more here.
Keywords:
mosi2 coatings;
sib6;
mosi2;
900 1200 ... See more keywords
Sign Up to like & get
recommendations!
0
Published in 2021 at "Advances in Materials Science and Engineering"
DOI: 10.1155/2021/9991967
Abstract: SiB6 powders were prepared by the “chemical oven” method from Si and B powders. Here combustion with acid pickling “two-step” mode replaces the traditional synthesis method which helps to avoid severe condition of high temperature…