Modeling and Simulation of Nanoindentation

Sign Up to like & get
recommendations!
Published in 2017 at "JOM"

DOI: 10.1007/s11837-017-2541-1

Abstract: Nanoindentation is a hardness test method applied to small volumes of material which can provide some unique effects and spark many related research activities. To fully understand the phenomena observed during nanoindentation tests, modeling and… read more here.

Keywords: simulation nanoindentation; modeling simulation; nanoindentation;