Sign Up to like & get
recommendations!
1
Published in 2017 at "Journal of Materials Science"
DOI: 10.1007/s10853-017-1833-8
Abstract: Recent advances in spherical nanoindentation protocols have proven very useful for capturing the grain-scale mechanical response of different metals. This is achieved by converting the load–displacement response into an effective indentation stress–strain response which reveals…
read more here.
Keywords:
spherical nanoindentation;
response;
indentation;
mechanical effects ... See more keywords
Sign Up to like & get
recommendations!
0
Published in 2017 at "Journal of Nuclear Materials"
DOI: 10.1016/j.jnucmat.2017.06.031
Abstract: Abstract Experimentally quantifying the mechanical effects of radiation damage in reactor materials is necessary for the development and qualification of new materials for improved performance and safety. This can be achieved in a high-throughput fashion…
read more here.
Keywords:
stress strain;
small scale;
spherical nanoindentation;
nanoindentation ... See more keywords