Published in 2020 at "Refractories and Industrial Ceramics"
DOI: 10.1007/s11148-020-00394-3
Abstract: AA7075-xZrB2 (x = 0, 5, 10, 15, and 20 wt.%) composites were manufactured by reacting potassium zirconium fluoride (K2ZrF6) and potassium tetrafluoroborate (KBF4) with molten AA7075 at 800°C. The ZrB2 particles formed by the reaction…
read more here.