Published in 2024 at "Advanced Engineering Materials"
DOI: 10.1002/adem.202401433
Abstract: ZGH451, a directionally solidified Ni‐based superalloy designed for additive manufacturing, has garnered significant attention in the realm of next‐generation turbine blades. Welding the ZGH451 superalloy is crucial for promoting its practical application. In this study,…
read more here.
Keywords:
superalloy;
liquid phase;
transient liquid;
zgh451 superalloy ... See more keywords
Photo from archive.org
Sign Up to like & get
recommendations!
1
Published in 2018 at "Oxidation of Metals"
DOI: 10.1007/s11085-017-9830-5
Abstract: Corrosion resistance of Inconel 625 Ni-based superalloy was studied in a molten nitrate salt consisting of 40 KNO3–60 NaNO3 (wt%) at 500 and 600 °C. Open-circuit potential, potentiodynamic polarization, electrochemical impedance spectroscopy and gravimetric tests were used…
read more here.
Keywords:
superalloy;
corrosion;
inconel 625;
molten nitrate ... See more keywords
Sign Up to like & get
recommendations!
0
Published in 2020 at "Tribology Letters"
DOI: 10.1007/s11249-020-1266-4
Abstract: Abstract The nickel-based single crystal (NBSC) superalloy has been widely used in aero engines, gas turbines, and other power plants due to its excellent high-temperature performance. During the working process, wear often occurs on the…
read more here.
Keywords:
temperature;
single crystal;
wear;
superalloy ... See more keywords
Sign Up to like & get
recommendations!
0
Published in 2018 at "Metallurgical and Materials Transactions B"
DOI: 10.1007/s11663-018-1256-1
Abstract: The influence of melt superheating treatment on the melt properties, solidification characteristics, and rupture life of a third-generation Ni-based single-crystal superalloy was investigated to reveal the critical temperature range of melt structure evolution and its…
read more here.
Keywords:
temperature;
life;
superalloy;
solidification characteristics ... See more keywords
Sign Up to like & get
recommendations!
0
Published in 2018 at "Rare Metals"
DOI: 10.1007/s12598-018-1093-z
Abstract: In the present investigation, a coupled crystal plasticity finite-element (CPFE) and cellular automaton (CA) model was developed to predict the microstructure of recrystallization in single-crystal (SX) Ni-based superalloy. The quasi-static compressive tests of [001] orientated…
read more here.
Keywords:
recrystallization;
single crystal;
superalloy;
model ... See more keywords
Sign Up to like & get
recommendations!
0
Published in 2018 at "Rare Metals"
DOI: 10.1007/s12598-018-1108-9
Abstract: Serrated flow phenomenon has been widely observed among different metals due to the potential influence on their applications. Uniaxial tensile tests of nickel-based superalloy GH536 were carried out at loading rates of 0.06, 0.60, 3.60,…
read more here.
Keywords:
serrated flow;
superalloy;
loading rates;
room temperature ... See more keywords
Sign Up to like & get
recommendations!
0
Published in 2018 at "Acta Metallurgica Sinica (English Letters)"
DOI: 10.1007/s40195-018-0705-9
Abstract: A modified FGH96 superalloy using 0.1 wt% graphene was successfully prepared using the wet mixing method. The interfacial bonding mechanism between the graphene and the superalloy matrix was characterized using optical microscope, scanning electronic microscope, transmission…
read more here.
Keywords:
mechanism graphene;
graphene;
superalloy;
interfacial bonding ... See more keywords
Sign Up to like & get
recommendations!
0
Published in 2019 at "Acta Metallurgica Sinica (english Letters)"
DOI: 10.1007/s40195-019-00891-6
Abstract: Both of the single crystal (SX) castability and undercoolability of PWA1383 superalloy were investigated during the directional solidification and isothermal cooling. In all the six SX parts of a casting cluster, no stray grains were…
read more here.
Keywords:
castability;
single crystal;
castability undercoolability;
undercoolability ... See more keywords
Sign Up to like & get
recommendations!
1
Published in 2020 at "Ceramics International"
DOI: 10.1016/j.ceramint.2020.07.157
Abstract: Abstract FGH96 is one kind of nickel-based superalloy, being widely used in aero engine hot end components due to its superior mechanical properties, while its machinability has been a challenge because of rapid tool wear…
read more here.
Keywords:
effects monolithic;
wear mechanisms;
ceramic tools;
superalloy ... See more keywords
Sign Up to like & get
recommendations!
1
Published in 2019 at "Corrosion Science"
DOI: 10.1016/j.corsci.2019.108127
Abstract: Abstract Three γ'-base coatings of Hf-doped and Re-modified NiCoCrAlTaY system were deposited on Rene N5 superalloy by magnetron sputtering. The cyclic oxidation behavior of these coatings was investigated at 1100 °C for 500 h. The γ'-base coatings…
read more here.
Keywords:
oxidation behavior;
superalloy;
cyclic oxidation;
base ... See more keywords
Photo from wikipedia
Sign Up to like & get
recommendations!
0
Published in 2020 at "International Journal of Fatigue"
DOI: 10.1016/j.ijfatigue.2019.105305
Abstract: Abstract Operating under elevated temperature and high stress for long terms, the regularly cubic γ ' precipitates of the Ni-based superalloy degrades to plate-like morphology perpendicular to the external stress. This process is called rafting…