Published in 2021 at "Journal of Alloys and Compounds"
DOI: 10.1016/j.jallcom.2021.158868
Abstract: Abstract In the present study, solid solution strengthened Ni-based superalloy Hastelloy X (HX) parts were fabricated using the laser powder bed fusion (LPBF) additive manufacturing process with the intent of developing a strong crystallographic texture.…
read more here.
Keywords:
orientation;
powder bed;
laser powder;
crystallographic orientation ... See more keywords