Sign Up to like & get
recommendations!
1
Published in 2019 at "Microscopy and Microanalysis"
DOI: 10.1017/s1431927619011620
Abstract: The nickel-base superalloy Inconel 718, have excellent properties to be used in high temperature applications, its principal characteristics are: high resistance to oxidation, good mechanical properties in elevated work temperatures, owing of that the principal…
read more here.
Keywords:
trace addition;
microstructure microhardness;
addition microstructure;
effect trace ... See more keywords
Sign Up to like & get
recommendations!
0
Published in 2020 at "Journal of Applied Physics"
DOI: 10.1063/5.0006006
Abstract: We present a broadband infrared and optical study of the compositionally complex nickel-based superalloy Inconel-718, a common material used in additive manufacturing using the direct metal laser sintering (DMLS) technique. We find a broad, featureless…
read more here.
Keywords:
inconel 718;
superalloy inconel;
based superalloy;
additive manufacturing ... See more keywords
Sign Up to like & get
recommendations!
0
Published in 2017 at "Materials Transactions"
DOI: 10.2320/matertrans.m2016376
Abstract: The morphological evolution of γ′ precipitates and lattice misfit with isothermal aging were closely investigated in wrought Ni-based superalloy Inconel X-750. The γ′ morphology dramatically changes in terms of shape, distribution, coalescence and coherency at…
read more here.
Keywords:
superalloy inconel;
evolution precipitates;
wrought based;
inconel 750 ... See more keywords
Sign Up to like & get
recommendations!
1
Published in 2020 at "Materials"
DOI: 10.3390/ma13235358
Abstract: Cyclic response and fatigue behavior are sensitive to the microstructure of material induced by heat treatment. In this paper, three sets of high-temperature superalloy Inconel 718 with different heat treatment, namely annealed, aged, and directly…
read more here.
Keywords:
heat treatment;
inconel 718;
superalloy inconel;
cyclic response ... See more keywords