Planar Front Growth of Single Crystal Ni-Based Superalloy René N515

Sign Up to like & get
recommendations!
Published in 2020 at "JOM"

DOI: 10.1007/s11837-020-04091-x

Abstract: A Ni-based superalloy, RenĂ© N515, was fabricated by the levitation zone melting process to produce planar front single crystal growth. Microstructure, alloy composition, and microhardness properties of the as-zone melted and solution heat treated alloy… read more here.