Published in 2023 at "Materials"
DOI: 10.3390/ma16103761
Abstract: The residual stress generated during heat treatment of nickel-base superalloys will affect their service performance and introduce primary cracks. In a component with high residual stress, a tiny amount of plastic deformation at room temperature…