Evolution of precipitates in Ni–Co–Cr–W–Mo superalloys with different tungsten contents

Sign Up to like & get
recommendations!
Published in 2020 at "Rare Metals"

DOI: 10.1007/s12598-020-01400-w

Abstract: The Ni–Co–Cr–W–Mo system is critical for the design of nickel-based superalloys. This system stabilizes different topologically close-packed (TCP) phases in many commercially superalloys with high W and Mo contents. Scanning electron microscopy (SEM), transmission electron… read more here.

Keywords: phase; thermodynamics; microscopy; precipitates superalloys ... See more keywords