Published in 2021 at "Nanoscale"
DOI: 10.1039/d1nr00447f
Abstract: Phase transformations occurring in a solid govern the structural and physical properties significantly. Nevertheless, deformation-induced phase transition in a soft-brittle solid has not been demonstrated yet. Soft-brittle cadmium zinc telluride (CZT) based instruments have produced…