Published in 2017 at "ACS applied materials & interfaces"
DOI: 10.1021/acsami.7b00427
Abstract: Many factors have been brought forward to explain the capacity degradation mechanisms of LiNixCoyMnzO2 (NCM)/graphite cells at extreme conditions such as under high temperature or with high cutoff voltage. However, the main factors dominating the…