Abstract: Abstract Crack formation in Si 3 N 4 active metal brazing (AMB) ceramic substrates and delamination of copper layers on the AMB substrates subjected to temperature cycling from −40 to 250 °C were investigated to evaluate…
read more here.
Keywords:
amb substrates;
crack formation;
thick layers;
copper ... See more keywords
Sign Up to like & get
recommendations!
0
Published in 2018 at "Journal of Solid State Chemistry"
DOI: 10.1016/j.jssc.2018.01.009
Abstract: Abstract A series of lanthanide coordination polymers LnBTPTA (Ln = Eu, Tb, EuxTb1−x), was synthesized using a tricarbocylic ligand 4,4′,4′′-(benzene-1,3,5-triyltris(1H-pyrazole-3,1-diyl))tribenzoic acid (H3BTPTA). X-ray single crystal analyses reveal that the asymmetric unit cell contains seven crystallographically…
read more here.
Keywords:
mixed lanthanide;
temperature;
thick layers;
coordination polymer ... See more keywords
Sign Up to like & get
recommendations!
0
Published in 2019 at "High Energy Chemistry"
DOI: 10.1134/s0018143919050059
Abstract: The influence of the conditions of mask-based photopolymerization of thick layers of a composition (with thickness h from 0.5 to 4.0 mm) based on dimethacrylate OCM-2 and o-quinone photoinitiator on the geometry of the resulting…
read more here.
Keywords:
photopolymerization thick;
mask based;
photopolymerization;
thick layers ... See more keywords