Published in 2020 at "Corrosion Science"
DOI: 10.1016/j.corsci.2020.108432
Abstract: Abstract Ferritic-Martensitic (F/M) steels with various amounts of alloying elements (Cr: 12 wt. %, Si: 0.6-2.2 wt. %, Mn: 0.6-1.8 wt. %) were exposed to Supercritical Water (SCW) environments at 500 °C and 25 MPa for up to 1000 hours. Gravimetric,…
read more here.
Keywords:
ferritic martensitic;
water;
martensitic steels;
corrosion ... See more keywords