Transient Liquid Phase Bonding of ZGH451 Superalloy Fabricated by Directed Energy Deposition

Sign Up to like & get
recommendations!
Published in 2024 at "Advanced Engineering Materials"

DOI: 10.1002/adem.202401433

Abstract: ZGH451, a directionally solidified Ni‐based superalloy designed for additive manufacturing, has garnered significant attention in the realm of next‐generation turbine blades. Welding the ZGH451 superalloy is crucial for promoting its practical application. In this study,… read more here.

Keywords: superalloy; liquid phase; transient liquid; zgh451 superalloy ... See more keywords